Media Blasting Services at DEK
Compressed air propels media at the machined surface, leaving a uniform, non-directional texture. Blasting is planned with the machining in the same order; no blasting-only orders.
What Media Blasting Delivers & Where to Be Mindful
Blasting changes texture and cleanliness, not geometry. Know its strengths and limits before you specify it on a machined part.
-
Key Benefits
- Tool marks disappear: cutter paths and step-over lines are replaced by a uniform, non-directional texture
- Hides fingerprints: the matte surface stays clean-looking on handled housings and hardware
- Light burrs removed: blasting knocks off light burrs left by machining
- Clean surface: scale, heat tint and EDM recast are cleaned off before the next finish
- Paint and powder key: aluminum oxide leaves an etched texture suited to paint adhesion
- Longer fatigue life: shot peening adds compressive stress 0.1–0.5 mm deep
-
Limitations & Alternatives
- No precision improvement: blasting does not improve flatness, roundness or Ra on a precision face
- Smooth or bright surface: choose polishing or electropolishing on stainless; blasting goes the other way
- Internal passages: blasting cannot reach cross-holes; see deburring for edge work inside
- Small parts in volume: vibratory tumbling gives a similar matte at lower cost per piece
- Material removal on fits: aluminum oxide removes 5–10 µm on aluminum, so tight bores need masking

Matte Finish and Surface Results
Each media gives a measurable result on a machined part: texture, roughness, cleanliness or fatigue resistance, matched to the next finish.
Blasting Media Compared
| Media | Grit / size | Resulting Ra | Effect on dimensions | Purpose and typical materials |
|---|---|---|---|---|
| Glass bead | #80–#170 | 0.8–1.6 µm | Negligible (< 2 µm) | Satin matte; cosmetic aluminum and stainless; pre-anodize; light peening |
| Ceramic bead | 60–150 µm | 0.4–1.0 µm | Negligible | Finer, brighter satin; consistent lot to lot; stainless, titanium, aluminum |
| Aluminum oxide | 60–220 grit | 1.5–4 µm | 5–10 µm removed on aluminum; edges rounded ~0.05 mm | Aggressive etch; paint/powder key; descaling; steel, titanium, cast iron |
| Steel shot | S110–S330 | 2–6 µm | Small growth, surface dimpled | Shot peening and descaling of steel; never on aluminum or stainless |
| Plastic media | Type II / Type V, 20–40 mesh | ≤ 0.8 µm | None | Gentle cleaning, paint stripping, deburring plastics and thin aluminum |
Suitable Materials for Media Blasting
Glass and ceramic bead suit aluminum, stainless steel and titanium; aluminum oxide and steel shot suit steel and cast iron.
Stainless and aluminum are never blasted or peened with steel media, to avoid iron contamination. Silica sand is not used: a “sandblasting CNC parts” note is treated as aluminum oxide or glass bead, confirmed at quote review.
-
6061 AluminumA #120 glass bead blast hides cutter paths before clear or black anodize; deoxidized before the bath.Recommended
-
6063 AluminumTakes the same even, low-gloss bead blast matte before anodizing as 6061 for cosmetic housings.Recommended
-
Stainless SteelGlass or ceramic bead gives a satin matte; peened with stainless, ceramic or glass media only.No steel media
-
TitaniumCeramic bead gives a bright, consistent satin; aluminum oxide etches it as a key under paint.Good
-
Alloy SteelAluminum oxide removes scale; cast steel shot S110–S330 is used for peening and descaling.Peening
-
Cast IronAluminum oxide gives an aggressive etch and scale removal ahead of paint or powder coat.Good
Typical Applications
Media blasting serves cosmetic aluminum hardware and fatigue-critical shafts and gears, from consumer electronics to aerospace landing gear.
Design & Tolerance Notes
Blasting reaches every exposed surface and can remove material, so the drawing must name the media, the surfaces, the masking and the follow-on finish.
-
Mask Critical Fits
Mask bores and shafts with H7/g6 or tighter fits, threads, sealing faces, O-ring grooves, lapped and datum faces, plus laser-marked zones.
-
Expect Edge Rounding
Unmasked aluminum oxide-blasted parts get a 0.05 mm edge radius; polished features lose some gloss.
-
Write the Drawing Note
Example: "Glass bead blast #120 all external surfaces; mask bore Ø12 H7, threads and face A". Add a boundary sample where cosmetic uniformity matters.
-
Name the Follow-On Finish
State "then anodize Type II clear" or "then passivate"; the same blast also works before black oxide on steel for a flat non-reflective black.
-
Sequence Peened Parts
Machine, heat treat, grind, peen, then plate or coat; a light polish may remove under 10% of the compressive depth.
-
Specify Shot Peening Services
Name the standard, media, Almen intensity, coverage and the peened surfaces on the drawing for shot peening services.
Blasting & Peening Specifications
- Glass bead grit #80–#170 (#120 general satin)
- Glass bead Ra 0.8–1.6 µm
- Ceramic bead Ra 0.4–1.0 µm
- Aluminum oxide removal 5–10 µm on aluminum
- Bead removal < 2 µm
- Peening depth 0.1–0.5 mm compressive
- Almen intensity 0.008–0.012 A / 0.006–0.010 N
- Coverage 100% min, 200% critical
- Peening standard AMS 2430 or SAE J2441
- Peened Ra 2–6 µm
- Feature tolerance ±0.005 mm
- Added lead time A day at most
- Certifications ISO 9001:2015, ISO 13485, AS9100D
Bead Blasting and the Shot Peening Process
Two processes with different goals: bead blasting for appearance before anodizing, peening for fatigue life.
Frequently Asked Questions
Answers on media choice, dimensions, anodizing and shot peening on machined parts.